3D print defect diagnosis

Pick the defect you see on your print. Each one lists the free checks to run in order, simplest first, and the full guide with causes and fixes. Defects covered: 12.

Adhesion and build plate

First layer not sticking or looking bad (too high, too squished, uneven)

Separate lines that peel off, a transparent scraped layer, areas that stick and others that don't: the cause is almost always a dirty plate, the wrong plate profile in the slicer or an incorrect nozzle-to-bed distance. Before buying a new plate, run these checks in order.

Quick checks (7)
  1. Do not touch the print surface with your fingers: skin oil is one of the most common causes of parts coming loose.
  2. Wash the plate when cold as the manufacturer recommends: Bambu Lab suggests warm water and dish soap without additives for textured PEI; Prusa uses isopropyl alcohol (~90%) for routine cleaning and water with dish soap when that is not enough. Never use acetone on textured plates.
  3. Check that the plate type selected in the slicer matches the plate installed and that the filament profile is correct (or a generic profile for the same material).
  4. Re-run calibration or automatic bed leveling, especially if the printer was moved or the bed removed; before leveling, make sure the nozzle is clean and properly secured.
  5. Adjust the Z offset (or Live Adjust Z on Prusa) in small steps: separate lines = nozzle too high; transparent layer or blocked extrusion = too low. Do not compensate for a dirty plate by squishing harder.
  6. If adhesion is still weak, raise the bed temperature slightly within the filament's range and slow down the first layer; add a brim for small parts.
  7. Only if one side of the plate has worn areas inside the print zone and the checks above do not help, use the other side or replace the plate.

Corners lifting off the bed (warping)

The corners of the part curl upward during printing, often on large flat parts or with high-shrinkage materials (ABS, ASA, PC, PA, but also PETG and PLA in cold rooms). Material shrinkage cannot be removed: it is reduced by improving adhesion and thermal stability.

Quick checks (7)
  1. Wash the plate as the manufacturer recommends and do not touch it with your fingers: a dirty plate makes corners lift even with correct settings.
  2. Eliminate drafts: windows, air conditioners and fans nearby cool one side of the part more than the other.
  3. With ABS, ASA and other engineering materials, close the door and lid of an enclosed printer and let the chamber warm up before starting; with PLA and PETG do not close the chamber unless the manufacturer says so (risk of extruder overheating).
  4. Use the filament profiles supplied with the slicer, then raise the bed temperature slightly within the recommended range.
  5. Add a brim, or 'ears' (brim ears / discs) only on the corners that lift.
  6. Adjust part cooling: low fan for ABS/ASA; for PLA and PETG Prusa suggests checking that the fan is on and increasing it if corners lift.
  7. For large flat parts reduce infill and choose a pattern that shrinks evenly (Bambu Lab suggests gyroid); apply a thin layer of glue stick if the manufacturer recommends it for that material.

Base of the part wider than the rest (elephant's foot)

The first layer sticks out from those above and parts do not fit together. It is usually caused by a first layer that is squished too much, a very hot bed or the slicer compensation: it is fixed with adjustments, without buying parts.

Quick checks (6)
  1. Clean and level the bed, then check that the first layer is not squished too much.
  2. Check the elephant's foot compensation in the slicer: Prusa gives about 0.2 mm for a 0.4 mm nozzle.
  3. For precision parts, measure the defect on a test cube and use the calculated value.
  4. Calibrate the filament flow if the first layer is over-extruded.
  5. Lower the bed temperature in 5 °C steps without compromising adhesion.
  6. Add a 45° chamfer to the bottom edge of the model.

Extrusion and filament

Clogged nozzle or under-extrusion

Thin or missing lines, layers with gaps, filament curling as it leaves the nozzle, an extruder that clicks or grinds the filament, or the printer moving with no material coming out. Before replacing the nozzle or hotend, find out where the blockage is: spool and PTFE tube, extruder (gears) or hotend/nozzle.

Quick checks (8)
  1. Make sure the spool turns freely, the filament is not tangled and the path to the extruder has no kinks or disconnected PTFE tubes.
  2. At printing temperature, extrude a little filament from the menu: if it comes out straight and steady the nozzle is not the problem; if it curls or struggles there is at least a partial clog.
  3. Separate extruder and hotend following your model's guide (pull the PTFE tube or remove the hotend and push filament through) to see where it stops.
  4. Clean filament dust off the extruder gears and check the idler tension: too loose slips, too tight grinds.
  5. With the nozzle hot, run the supplied cleaning needle through it without pushing it deep, then do one or more cold pulls until the extracted tip comes out clean.
  6. Rule out heat creep: heatsink fan working and clean, enclosure not too hot when printing PLA, bed no hotter than needed.
  7. If the filament crackles or bubbles, dry it before looking for mechanical faults.
  8. Replace the nozzle, PTFE tube or gears only if cleaning and cold pulls don't help or the part is visibly damaged or worn.

Wet filament

Popping or hissing during extrusion, bubbles and small holes, stringing and oozing, a rough surface, weaker parts. Many filaments absorb moisture from the air; nylon (PA), TPU and PVA/BVOH are among the most sensitive, but PETG and PLA can be affected too. It often looks like a printer fault: before replacing parts, dry the filament following the manufacturer's guidance.

Quick checks (6)
  1. Listen to the nozzle while extruding: popping, crackling or small puffs of steam almost always mean wet filament.
  2. Extrude some filament by hand and look at it: bubbles or a rough, uneven surface are a typical sign.
  3. Print the same file with a freshly opened or already dried spool, changing nothing else: if the defect disappears, the filament is the cause.
  4. Dry it following the filament or printer manufacturer's table, staying within the spool's maximum temperature; never use a microwave.
  5. After drying, store the spool in a sealed container with desiccant and a hygrometer; regenerate or replace the desiccant once it has changed colour.
  6. If defects persist with dry filament, check retraction, temperature and nozzle before considering replacement parts.

Thin strings between parts (stringing) and blobs of material (oozing)

Cobweb-like strands between parts of the model, blobs or drips on the nozzle during travel moves. It usually comes from wet filament, a nozzle temperature that is too high or unsuitable retraction: it can almost always be fixed with checks and adjustments, without buying parts.

Quick checks (7)
  1. Make sure the material profile and nozzle diameter selected in the slicer really match the filament and nozzle installed.
  2. Try another spool or dry the one in use: wet filament strings even with correct settings (see the filament drying guide).
  3. Clean material residue off the nozzle while hot, with proper protection against burns.
  4. Lower the nozzle temperature in small steps, staying within the range given by the filament manufacturer.
  5. Check retraction (length, speed, travel threshold): start from the official profile values and change one parameter at a time.
  6. Enable "wipe while retracting" and the option that avoids crossing perimeters/walls; place models closer together on the plate.
  7. If strings persist with dry filament and a correct profile, check nozzle wear and the condition of the PTFE tube and extruder gears.

Layers separating or cracking (delamination)

Horizontal cracks along the walls or layers coming apart, especially on tall or large parts and with ABS and ASA. It is usually caused by a temperature that is too low, too much cooling or draughts: it is fixed with settings, without buying parts.

Quick checks (6)
  1. Check that the material profile in the slicer matches the loaded filament.
  2. Raise the nozzle temperature in 5 °C steps, staying within the range printed on the spool.
  3. With ABS and ASA, reduce or switch off the part cooling fan, keep the printer closed and avoid draughts.
  4. Keep the layer height below about 80% of the nozzle diameter.
  5. Reduce the wall speed and increase the number of perimeters.
  6. Try another spool and check that the nozzle is not partially clogged.

Motion and surface quality

Shifted layers: the model suddenly "steps" along X or Y

At a certain height all following layers are offset along the X or Y axis. The most common causes are loose or over-tight belts, loose pulleys, the nozzle hitting curled-up parts, obstructions to movement and excessive speed or acceleration. It can almost always be fixed with mechanical and settings checks.

Quick checks (8)
  1. With the printer off and cool, move the toolhead and bed by hand: they must glide without tight spots; look for cables, PTFE tubes, filament or debris obstructing movement.
  2. Look at the model: if there are overhangs or curled edges, the nozzle may be hitting them; improve adhesion and cooling and consider Z hop.
  3. Check belt tension using the manufacturer's procedure: neither slack nor tight like a guitar string.
  4. Make sure the grub screws on the motor pulleys are tight, with one sitting on the flat of the shaft.
  5. Restore speed and acceleration to the official profile values; on Prusa use normal mode instead of stealth mode for large prints.
  6. Clean and lubricate rails and rods as described in the manual; repeat vibration (input shaping) calibration if available.
  7. Check that the electronics ventilation openings are not clogged with dust: overheating drivers can lose steps.
  8. Only after all these checks suspect the motor, cable or mainboard, and follow the manufacturer's diagnostic procedure.

Ringing / ghosting: ripples and “echoes” on walls after corners and lettering

Ripples that repeat a corner, hole or embossed text a few millimetres further along the wall. They are machine vibrations after fast direction changes: loose belts, loose parts, an unstable surface, excessive acceleration or out-of-date vibration compensation (input shaping). Fix the mechanics first, then recalibrate.

Quick checks (7)
  1. Place the printer on a rigid, stable surface; remove things that rattle (spool holder, cables, panels) and make sure all feet touch down.
  2. With the printer off and cool, check frame, toolhead and bed screws: no play and no parts that move by hand.
  3. Check belt tension with your printer's official procedure (spring tensioner, measuring app or calibration): neither loose nor overtightened.
  4. Clean and lubricate rails and rods as the manual says; on machines with eccentric wheels, adjust the wheels until there is no play.
  5. Rerun vibration calibration (input shaping / resonance compensation) after any mechanical work, with the machine standing still on a stable surface.
  6. If ringing remains, lower outer-wall acceleration and speed in the slicer and compare on a simple test print.
  7. If calibration still reports abnormal frequencies after these checks, inspect pulleys and motors: replace only damaged belts or bearings.

Overhangs and bridges that sag or curl

Curled edges, rough surfaces or strands hanging under overhanging sections. It usually depends on cooling, speed or temperature; beyond a certain angle you need supports. It is fixed with settings, without buying parts.

Quick checks (6)
  1. Check that the part cooling fan works and that the air duct is not blocked.
  2. Increase the fan on bridges and overhangs, moderately for ABS, ASA and PC.
  3. Keep overhang slowdown enabled or reduce the outer wall speed.
  4. Lower the nozzle temperature in 5 °C steps.
  5. Reduce the layer height where the overhangs are.
  6. Use supports or rotate the part for angles that remain defective.

Visible seam or zits on walls

A vertical line on the wall or lots of small dots where each perimeter starts and ends. The seam cannot be eliminated completely, but it can be hidden with the right position in the slicer, flow calibration and dry filament, without buying parts.

Quick checks (5)
  1. Choose the seam position for the part: “Aligned” or “Nearest” with corners, “Back” to hide it on the back.
  2. Avoid “Random” on parts with corners: it leaves small zits all over the surface.
  3. On curved surfaces, try the scarf seam if your slicer offers it.
  4. Calibrate flow and pressure advance (Linear Advance or Flow Dynamics) for the filament you use.
  5. If large or irregular blobs appear, dry the filament.

Holes or dips in the top surface (pillowing)

The top face of parts ends up full of holes, rough or bulging between the infill lines. It usually depends on too few top layers, infill that is too sparse or insufficient cooling: it is fixed with settings, without buying parts.

Quick checks (5)
  1. Increase the top layers: at least 3, more with thin layers.
  2. Increase the infill if it is below 10–15%, or make it denser only under the top surface.
  3. Check that the part cooling fan works and that the duct is not blocked.
  4. If holes appear everywhere, check flow and nozzle to rule out under-extrusion.
  5. In PrusaSlicer, keep “Ensure vertical shell thickness” enabled for sloping surfaces.